26. March 2022
DIFENDER – Now approved according TL 2350-0000
Our DIFENDER special steel is your best choice when you need to meet ultra-high security requirements with the minimum of weight. DIFENDER protects civilian and military armoured land vehicles and water craft, cash transporters and buildings against ballistic and explosive attack.
DIFENDER offers:
- excellent resistance against bullet, blast waves impact and splittering in combination with high hardness, strength and low weight
- hardness values of 400, 450, 500 and 600 HBW
- good impact values (longitudinal and transverse) at -40 °C
- thickenesses up to 150 mm
- thickness tolerances: -0/+0,8 mm
- restricted flatness tolerances acc. tab. 5 EN 10029
- specific testing on mother plate with 3.1 material test report
- good processing properties
- now also approval according the German Army standard TL 2350-0000
The distribution of DIFENDER is done via direct sales or specialized Steel Service Centers, even small orders.
Christoph Dickmann
Head of Sales Department, Machinery & Construction Equipment, Protection Steel
Phone: +49 6831 472385
Fax: +49 6831 47992681
E-Mail
Dr. Axel Grüneklee
Category Manager Sales, Protection Steel
Phone: +49 6831 475791
E-Mail
Johannes Klemm
Head of Marketing & Technical Support, Machinery & Construction Equipment, Steel Service Center, Plate Processing, Protection Steel
Phone: +49 6831 475658
Fax: +49 6831 47999036
E-Mail