High-temperature steels
For lasting durability at elevated temperatures
Dillinger's high-temperature steels in conformity to the EN 10028, Part 2, standard or the corresponding ASME standards are the right choice if your steam boilers, pressure vessels or pipes are continuously exposed to elevated temperatures.
The Dillinger range for your needs
- Dillinger has many years of international experience in the supply of high-temperature steels, such as its CrMo(V) grades for the petrochemicals industry.
- We can meet the most demanding customer specifications.
- Our alloyed and non-alloy steels possess high high-temperature yield strengths and long-term properties. The processes used for their production make them resistant to failure mechanisms typical in such applications, such as hydrogen embrittlement and temper embrittlement.
- You also benefit from good weldability, the result of these steels' optimised chemical composition.