S500G1+M/G2+M

Offshore steel with high minimum yield strength for lower weights

Our S500G1+M/G2+M proprietary steel is the right choice wherever extremely high requirements are made for weight-savings, weldability and safety – in the construction of offshore rigs, for example.

The strengths of S500G1+M/G2+M proprietary steel

  • This thermomechanically rolled fine-grained structural steel permits weight reductions thanks to its high and constant minimum yield strengths in the respective dimensions range: 500 MPa in 10 to 75 mm thicknesses, and 480 MPa in 75 to 100 mm thicknesses.
  • S500G1+M/G2+M is based on the NORSOK MDS Y50/Y55 standard and thus also meets toughness requirements at half plate thickness.
  • S500G1+M/G2+M can be supplied in the form of “pre-qualified material” with corresponding weldability analysis certificates.

Applications

Downloads

Data sheets & specifications

D-PURE+ – Heavy plate with a reduced CO2 footprint
DILLIDUR 325 L – Air hardened wear resistant steel
DILLIMAX 690 – High strength fine grained structural steel, quenched and tempered
DILLIMAX 890 – High strength fine grained structural steel, quenched and tempered
DILLIMAX 1100 – High strength fine grained structural steel, quenched and tempered
DILLIMAX 965 – High strength fine grained structural steel, quenched and tempered
DILLIMAX 890 – High strength fine grained structural steel, quenched and tempered
DILLIDUR 450 – Wear resistant steel
DILLIDUR 500 – Wear resistant steel
DILLIDUR 400 – Wear resistant steel
DILLIDUR 600 – Wear resistant steel
DILLIDUR IMPACT – Wear resistant steel
DILLIDUR 550 – Wear resistant steel
DILLIMAX & DILLIDUR – Ultra high strength and wear resistant plates from Dillinger
DILLIMAX & DILLIDUR – a brief overview
Delivery program – heavy plate
DILLIMAX 550 – High strength fine grained structural steel, quenched and tempered
DILLIMAX 500 – High strength fine grained structural steel, quenched and tempered
DICUT – Heavy plates with improved laser cutting properties
OFL-L – Plates with high surface quality for lift arms
DILLIMAX TL – High yield strength fine grained structural steels with close tolerances on dimension and shape

Processing information

DILLIDUR Processing information: properties
DILLIDUR Processing information: properties
DILLIMAX Processing information: properties
DILLIMAX Processing information: machining
DILLIMAX Processing information: cutting
DILLIMAX Processing information: properties
DILLIMAX Processing information: welding
DILLIDUR Processing information: machining
DILLIMAX Processing information: welding
DILLIDUR Processing information: welding
DILLIDUR Processing information: welding
DILLIMAX Processing information: cutting
DILLIDUR Processing information: forming
DILLIMAX Processing information: forming
DILLIDUR Processing information: cutting
DILLIDUR Processing information: cutting

Contact

20230731100229-domin

Lutz Domin
Head of Sales Department Steel Service Center, Plate Processing

Phone: +49 6831 472195
Fax: +49 6831 474580
E-Mail

20221012111603-klemm_2022

Johannes Klemm
Head of Marketing & Technical Support, Machinery & Construction Equipment, Steel Service Center, Plate Processing, Protection Steel

Phone: +49 6831 475658
Fax: +49 6831 47999036
E-Mail