Dillinger heavy plate for the
Hollandse Kust West offshore wind farm
Energy of the future – Hollandse Kust West VI & VII driving the energy transition forward
The two wind farms, Hollandse Kust West VI (Ecowende) and Hollandse Kust West VII (OranjeWind), will be constructed around 53 kilometres off the Dutch coast near IJmuiden. They are considered two major projects in the expansion of the Netherlands’ renewable energy infrastructure.
With 52 wind turbines, the Hollandse Kust West VI wind farm achieves a total production capacity of around 760 MW, enough clean energy to cover about 3% of the current Dutch electricity demand.
During the planning and construction of the wind farm, particular attention is being paid to preserving a thriving ecosystem, whilst keeping the impact on birds, bats and the underwater world to a minimum.
The neighbouring Hollandse Kust West VII wind farm consists of 53 wind turbines and, with a total capacity of 795 MW, can generate around 3 TWh per year. This corresponds to the annual electricity consumption of more than one million Dutch households. It thus achieves a similar level of supply performance as Hollandse Kust West VI.
Both offshore wind farms are built on monopile foundations, which are securely anchored at water depths of 26 to 33 m.
For these two impressive projects, Dillinger supplied around 135,535 tonnes of heavy plate in the offshore steel grades S355ML, S355MLO and S420ML, in thicknesses ranging from 25 to 114 mm.
Offshore substations – Efficient power transmission with Dillinger steel
The two substations, Hollandse Kust West Alpha and Hollandse Kust West Beta, form another significant part of the Netherlands’ offshore infrastructure. They are located approximately 50 and 53 kilometers off the Dutch coast in the North Sea near Egmond aan Zee.
Their function is to collect the energy generated by the wind turbines in the wind farms and convert it from a lower to a higher voltage in order to transport the electricity efficiently to shore.
Hollandse Kust West Alpha consists of a topside weighing over 3,600 tonnes, installed on a jacket platform weighing around 2,400 tonnes.
A similar structure was also implemented for Hollandse Kust West Beta. The first milestone in its construction was reached in mid-2024, when the approximately 49-meter-long and over 2,100-tonne foundation structure, the jacket, was safely placed on the seabed. This was followed by the installation of the roughly 4,000-tonne topside. The installation was carried out by the heavy-lift vessel SSCV Sleipnir, which positioned the jacket and the topside in precise lifting operations.
For both substations, the jacket foundations were secured at the four corners with piles (so-called pin piles), which extend more than 50 m into the seabed, thus ensuring secure anchoring.
With a total capacity of 700 MW each, both plants make a significant contribution to the Netherlands’ sustainable energy supply.
Dillinger contributed to these renewable energy projects by supplying around 2,530 tonnes of demanding offshore steel grades, such as the high-strength S460MLO grade, as well as plates with widths of over 4 metres.