Dillinger heavy plate for the new Etzel-Wardenburg natural gas pipeline

A contribution to the security of supply of natural gas in Germany

Open Grid Europe (OGE) is building a natural gas pipeline from Etzel via Wardenburg to Drohne to expand its supra-regional long-distance gas transportation system. The north-south pipeline consists of the two pipeline sections from the storage facility in Etzel to the compressor station in Wardenburg (EWA) and from Wardenburg to Drohne (WAD). In total, the pipeline measures approx. 138 kilometers and has a diameter of DN 1200 mm and DN 1000 mm respectively. The new pipelines will create the necessary transport capacity to transport the liquefied gas that arrives in Wilhelmshaven into the German natural gas pipeline network, thereby making a significant contribution to the security of natural gas supplies in Germany. The new Etzel-Wardenburg-Drohne project will ensure the supra-regional supply of consumers and industry.

The two pipeline sections are scheduled for completion by the end of 2026 and 2027 respectively.

The EUROPIPE plant in Mülheim, a company of the Dillinger Group, is building these large-diameter pipes, which are also certified for the transportation of hydrogen, to enable the transportation of alternative energies. Dillinger supplied 28,500 tons of L485ME grade steel in widths greater than 3.5 m for the production of the longitudinally welded large-diameter pipes for the Etzel-Wardenburg pipeline section.

oge_1
oge_leitungsnetzkarte_de-2

Data

Building owner
Open Grid Europe (OGE)
Project partner
EUROPIPE-Werk Mülheim
Product type
Erdgasleitung
Installation
End of 2026
Country
Germany
Quality
L485ME
Length
138 km
Width
> 3.5 m
Diameter
DN 1200 mm
Tonnage
28,500 t

Contact persons

20200128093033-ludwig_p_2020

Philipp Ludwig
Sales Director
Energy Transmission & Processing, H2 Infrastructures

Phone: +49 6831 472472
Fax: +49 6831 47992685
E-Mail

20221012121114-maffert_2022

Jörg Maffert
Strategy & Marketing,
Head of Energy

Phone: +49 6831 473612
E-Mail